Wear rate of PMMA and UHWPE reinforcement with $SiO_2$ nano fillers | ||
| International Journal of Nonlinear Analysis and Applications | ||
| مقالات آماده انتشار، اصلاح شده برای چاپ، انتشار آنلاین از تاریخ 20 تیر 1405 اصل مقاله (1.4 M) | ||
| نوع مقاله: Research Paper | ||
| شناسه دیجیتال (DOI): 10.22075/ijnaa.2024.35354.5263 | ||
| نویسندگان | ||
| Hoda Doostmohammadi1؛ Nima Refahati* 2 | ||
| 1Department of Mechanical Engineering, Damavand Branch, Islamic Azad University, Damavand, Iran. | ||
| 2Department of Mechanical Engineering, Damavand Branch, Islamic Azad University, Damavand, Iran | ||
| تاریخ دریافت: 27 خرداد 1403، تاریخ بازنگری: 17 مهر 1403، تاریخ پذیرش: 18 مهر 1403 | ||
| چکیده | ||
| Improving the quality of biomaterials and increasing their durability has always been one of the significant concerns in biomechanical studies. The use of nano-polymers may enhance the properties of implants and biomaterials. The purpose of this paper is to evaluate the influences of adding a different percentage of $Sio_2$ nanoparticles on wear resistance refinement. To measure the impacts of $ SiO_2$ nanoparticles on wear resistance, reinforced PMMA and UHWPE with Nano $SiO_2$ powders were produced. The effect of 0%,3%, and 5% Mass fraction of $SiO_2$ fillers on the wear rate of UHWPE as the artificial joint and 0%,3%, 5%, and 7% fraction of $SiO_2$ fillers on the wear rate of PMMA denture base, experimented by wear machine Tuber GT-7012-T according to ASTM 99g 2017. The experimental results demonstrate that at 5% mf of Nanoparticles, the wear rate reduces up to 40%. However, increasing the mf of Nanoparticles is improper and decreases the wear resistance. One-way ANOVA analysis was applied to determine significant differences between data. | ||
| کلیدواژهها | ||
| PMMA؛ UHWPE؛ Nano Fillers؛ Wear test؛ denture | ||
| مراجع | ||
|
[1] O. Alharba, H. Akilb, and Z. Ahmadc, Influence of Al2O3/Y‑TSZ mixture as filler loading on the radiopacity of PMMA denture base composites, Procedia Chem. 19 (2016), no. 4, 646-650. [2] A. Alhotan, J. Yates, S. Zidan, J. Haider, and N. Silikas, Flexural strength and hardness of filler‑reinforced PMMA targeted for denture base application, Materials 14 (2021), no. 10, 2659. [3] Alqahtani, Mechanical properties enhancement of self‑cured PMMA reinforced with zirconia and boron nitride nanopowders for high‑performance dental materials, J. Mech. Behav. Biomed. Mater. 110 (2020), no. 2, 103937. [4] S. An, J.L. Evans, S. Hamlet, and R.M. Love, Overview of incorporation of inorganic antimicrobial materials in denture base resin: A scoping review, J. Prosth. Dent. 130 (2023), no. 2, 202-211. [5] H. Azlina, J. Hasnidawani, H. Norita, and S. Surip, Synthesis of SiO2 nanostructures using Sol‑Gel method, Acta Phys. Polonica A 129 (2016), no. 4, 842-844. [6] Ch.R. Bragdon, D.O. O'Connor, J.D. Lowenstein, M. Jasty, S.A. Biggs, and W.H. Harris, A New Pin‑on‑Disk Wear Testing Method for Simulating Wear of Polyethylene on Cobalt‑Chrome Alloy in Total Hip, J. Arthropl. 16 (2001), no. 5, 658-666. [7] A. Cahyanto, M.V. Martins, O. Bianchi, D.P. Sudhakaran, N. Silikas, S.G. Echeverrigaray, and V. Rosa, Graphene oxide increases PMMA's resistance to fatigue and strength degradation, Dental Mater. 39 (2023), no. 9, 763-769. [8] N.W. Elshereksi, A. Muchtar, and C.H. Azhari, Effects of nanobarium titanate on physical and mechanical properties of poly (methylmethacrylate) denture base nanocomposites, Polym. Polym. Compos. 29 (2021), no. 4, 484-496. [9] G. Ergun, Z. Sahin, and A.S. Ataol, The effects of adding various ratios of zirconium oxide nanoparticles to poly (methyl methacrylate) on physical and mechanical properties, J. Oral Sci. 60 (2018), no. 8, 304-315. [10] A.A. Fatalla, M.S. Tukmachi, and G.H. Jani, Assessment of some mechanical properties of PMMA/silica/zirconia nanocomposite as a denture base material, IOP Conf. Ser.: Mater. Sci. Engin.: IOP Pub. 987 (2020), no. 1, 12031. [11] M.A. Golshokouh, N. Refahati, and P.R. Saffari, Effect of silicon nanoparticles on moisture absorption and fracture toughness of polymethyl methacrylate matrix nanocomposites, J. Compos. Sci. 8 (2024), no. 2, 69-80. [12] K. Gonga, B. Luo, B. Di Feng, and L. Changhai, Wear of Ni3Al‑based materials and its chromium‑carbide reinforced composites, Wear 265 (2008), no. 11, 1751-1755. [13] N.A. Hassan, J.N. Hasnidawani, N. Hassan, and S.N. Surip, Synthesis of SiO2 nanostructures using sol‑gel method, Acta Phys. Polonica 129 (2016), no. 4, 842-844. [14] A. Hasanen and M. Mudhafter, The effect of Silicon dioxide Nano‑Fillers reinforcement on some properties of heat cure polymethyl methacrylate, J. Bagh College Dent. 26 (2014), no. 10, 32-36. [15] L. Kang, A.L. Galvin, T.D. Brown, J. Fisher, and Z.M. Jin, Wear simulation of ultra‑high molecular weight polyethylene hip implants by incorporating the effects of cross‑shear and contact pressure, J. Engin. Med. 222 (2007), no. 8, 1049-1065. [16] Sh.H. Kenneth, M. Warren, W. Corrine, and H. Hacker, In vitro wear of resin denture teeth, J. Prosth. Dent. 79 (1998), no. 2, 152-158. [17] D.W. Lee and B.R. Yoo, Advanced silica/polymer composites: Materials and applications, J. Ind. Engin. Chem. 38 (2016), no. 11, 1-12. [18] T. Liu, B. Li, B. Lively, A. Eyler, and W.H. Zhong, Enhanced wear resistance of high‑density polyethylene composites reinforced by organosilane‑graphitic nanoplatelets, Wear 309 (2009), no. 1, 43-51. [19] T.K. McGloughlin and A.G. Kavanagh, Wear of ultra‑high molecular weight polyethylene (UHMWPE) in total knee prostheses: a review of key influences, Proc. Instn. Mech. Engrs. 214 (2000), no. 4, 349-359. [20] V. Preis, S. Hahnel, M. Behr, and M. Rosentritt, Contact wear of artificial denture teeth, J. Prosthod. Res. 62 (2017), no. 2. [21] J. Slane, J. Vivanco, J. Meyer, H.L. Ploeg, and M. Squire, Modification of acrylic bone cement with mesoporous silica nanoparticles: Effects on mechanical, fatigue and absorption properties, J. Mech. Behav. Biomed. Mater. 29 (2014), no. 1, 451-461. [22] F.J. Tommasini, L.D. Ferreira, L.G. Tienne, V.D. Aguiar, M.H. Silva, L.F. Rocha, and M.D. Marques, Poly (methyl methacrylate)‑SiC nanocomposites prepared through in situ polymerization, Mater. Res. 21 (2018), no. 6, e20180086. [23] D. Tzetzis, K. Tsongas, and G. Mansour, Determination of the mechanical properties of epoxy silica nano composites through FEA‑supported evaluation of ball indentation test results, Mater. Res. 20 (2017), no. 10, 1571-1578. [24] M.S. Zafar, Prosthodontic applications of polymethyl methacrylate (PMMA): An update, Polymers 12 (2020), no. 10, 2299. [25] C. Zietz, J. Reinders, J. Schwiesau, A. Paulus, J.Ph. Kretzer, T. Grupp, S. Utzschneider, and R. Bader, Experimental testing of total knee replacements with UHMW‑PE inserts: Impact of severe wear test conditions, Clinic. Appl. Biomater. 26 (2015), no. 3, 133-146. | ||
|